Default magazine and gorilla glue

stopped at store to get somethings and happen want to check magazine, on peterson's bow and arrow magazine they are endrose gorilla glue for arrow building and it's show couple od advertise of gorilla glue on magazine

i think gorilla going to be top notch for carbon arrow ..
JTClark is offline   Reply With Quote
Old 02-05-2011, 10:39 PM   #2
elkslayer4x5
EastOutfitters
 
elkslayer4x5's Avatar
 
Join Date: Apr 2008
Location: Lane County, Oregon
Posts: 288
elkslayer4x5 is on a distinguished road
Default

Will it heat release if you should need to pull an insert? If you see no need to unassemle an arrow, why not, I think most clues we use now are various super glue fomulas.
__________________
Visit our web site
http://eastoutfitter.tripod.com/index.html
2 06 Martin Slayers, 63 & 55#s Nitrous C X QuikTune 3000s and HHA OL 5519s on both.
04 Martin Cougar Elite Nitrous C X Quiktune 1000
elkslayer4x5 is offline   Reply With Quote
Old 02-06-2011, 12:06 AM   #3
Deadeyerick
Junior Member
 
Deadeyerick's Avatar
 
Join Date: Apr 2006
Location: Downers grove, IL
Posts: 25
Deadeyerick is on a distinguished road
Send a message via AIM to Deadeyerick
Default

I use gorilla glue super glue to fletch arrows. Works great and it is a lot cheaper than Tim's Goat Tough. It is just another cyanoacrylate glue. I do not think regular Gorilla Glue would work very well
Deadeyerick is offline   Reply With Quote
Old 02-06-2011, 03:32 AM   #4
Daniel Boone
Senior Member
 
Daniel Boone's Avatar
 
Join Date: May 2006
Posts: 6,934
Daniel Boone is on a distinguished road
Default Regular

Quote:
Originally Posted by Deadeyerick View Post
I use gorilla glue super glue to fletch arrows. Works great and it is a lot cheaper than Tim's Goat Tough. It is just another cyanoacrylate glue. I do not think regular Gorilla Glue would work very well
I tried some of the regular stuff and it dont work. Must be this super glue.
DB
__________________
Elite bows, Vortex Binos, Trophy Taker sights, Carter releases, Goldtip Arrows. CBE sights, Vapor Trail Strings, B Stinger stabilizers
Daniel Boone is offline   Reply With Quote
Old 02-06-2011, 10:27 AM   #5
MeanV2
Senior Member
 
MeanV2's Avatar
 
Join Date: Jul 2007
Location: SE Illinois
Posts: 1,162
MeanV2 is on a distinguished road
Default

For fletching I prefer the Fletch Tite Platinum, and gluing inserts in I prefer the Easton HIT epoxy. Slower set but stronger bond & less brittle than other epoxies.

It is what it was designed for

Dan
__________________
Maker of MEANV STRING SUPPRESSORS
MAITLAND BOW DEALER
Dealer for Slick Tricks, Vapor Trail Limb Driver & Strings, HHA sights, Viper Sights, etc.
www.meanvarchery.com
MeanV2 is offline   Reply With Quote
Old 02-06-2011, 10:32 AM   #6
Hoyt1945
Senior Member
 
Join Date: Nov 2008
Posts: 183
Hoyt1945 is on a distinguished road
Default

There has been a lot of discussion on glues for arrow making. Here is my 2 cents worth. Two choices for fletching, super glue regardless of brand since it is all cyanoacylate and bohning fletch-tite-platinum. For inserts low-temp hot melt. I personally like the fletch-tite platinum, but will use super glue on occasion. I do a lot of tinkering with point weight and with low temp hot melt you can remove points with ease. I use to use expoxy and I think I lost more point with expoxy. Don't remember leaving an insert in the bale using hot melt.
__________________
Hoyt Bows, Shrewd sights, Carter index, Tru Ball hinge, Trophy Taker Rest, Doinker Stabilizers, Carbon Express XJ 27's, Vapor Trail Strings, Nikon Binos.
Hoyt1945 is offline   Reply With Quote
Old 02-06-2011, 10:51 AM   #7
MeanV2
Senior Member
 
MeanV2's Avatar
 
Join Date: Jul 2007
Location: SE Illinois
Posts: 1,162
MeanV2 is on a distinguished road
Default

I understand that and that's the reason I say if a person is going to use Epoxy they are better using the slow set epoxies. IMO they are less brittle and not as prone to breaking loose

Dan



Quote:
Originally Posted by Hoyt1945 View Post
I use to use expoxy and I think I lost more point with expoxy.
__________________
Maker of MEANV STRING SUPPRESSORS
MAITLAND BOW DEALER
Dealer for Slick Tricks, Vapor Trail Limb Driver & Strings, HHA sights, Viper Sights, etc.
www.meanvarchery.com
MeanV2 is offline   Reply With Quote
Old 02-06-2011, 11:59 AM   #8
Hoyt1945
Senior Member
 
Join Date: Nov 2008
Posts: 183
Hoyt1945 is on a distinguished road
Default

Quote:
Originally Posted by MeanV2 View Post
I understand that and that's the reason I say if a person is going to use Epoxy they are better using the slow set epoxies. IMO they are less brittle and not as prone to breaking loose

Dan
You may have a point there, I live in a small town and all I have found is a fast curing expoxy, It seem everybody wants the fast drying stuff. It isvery brittle when it dries. Next order to Lancaster I my order some the easton epoxy. Knock on wood, but I have had good success with low temp hot melt.
__________________
Hoyt Bows, Shrewd sights, Carter index, Tru Ball hinge, Trophy Taker Rest, Doinker Stabilizers, Carbon Express XJ 27's, Vapor Trail Strings, Nikon Binos.
Hoyt1945 is offline   Reply With Quote
Old 02-06-2011, 01:51 PM   #9
JTClark
Senior Member
 
Join Date: Jan 2011
Location: Wisconsin
Posts: 199
JTClark is on a distinguished road
Default

hotmelt that they say it work that is what they use for point weight at 3d shooting but i'm not the 3d but a hunting and shoot backyard it all so all i can do is get a gold tip grip glue, if i want to aligment my head i would might use hotmelt but RISK for sure..
JTClark is offline   Reply With Quote
Old 02-06-2011, 02:10 PM   #10
stealthshooter
Junior Member
 
Join Date: Jan 2009
Posts: 10
stealthshooter is on a distinguished road
Default

I use the Gorilla super glue for fletching and I love it! It has a rubber additive that helps it flex a bit. I use epoxy or hot melt for the inserts.
stealthshooter is offline   Reply With Quote
Old 02-06-2011, 07:07 PM   #11
JTClark
Senior Member
 
Join Date: Jan 2011
Location: Wisconsin
Posts: 199
JTClark is on a distinguished road
Default

bought a bowhunter magazine and show adversite of gorilla glue, i guess they are start carry gorilla out and i'm sure gorilla will make a glue, fletching for archery, so if u are get magazine every month check ur magazine..
JTClark is offline   Reply With Quote
Old 02-07-2011, 09:02 AM   #12
Gator eye
Senior Member
 
Gator eye's Avatar
 
Join Date: Jul 2007
Location: In the horn of Michigan
Posts: 7,185
Gator eye is a jewel in the roughGator eye is a jewel in the roughGator eye is a jewel in the roughGator eye is a jewel in the rough
Default

I tried the gorillla super glue for fletching but it leaves a white film on the arrows, which I didn't like. I went back to fletch tite platinum.
Gator eye is offline   Reply With Quote
Old 02-07-2011, 09:17 AM   #13
MeanV2
Senior Member
 
MeanV2's Avatar
 
Join Date: Jul 2007
Location: SE Illinois
Posts: 1,162
MeanV2 is on a distinguished road
Default

That's one reason I like the Fletch Tite also.

Trivial I know!

Dan



Quote:
Originally Posted by Gator eye View Post
I tried the gorillla super glue for fletching but it leaves a white film on the arrows, which I didn't like. I went back to fletch tite platinum.
__________________
Maker of MEANV STRING SUPPRESSORS
MAITLAND BOW DEALER
Dealer for Slick Tricks, Vapor Trail Limb Driver & Strings, HHA sights, Viper Sights, etc.
www.meanvarchery.com
MeanV2 is offline   Reply With Quote
Old 02-07-2011, 11:51 AM   #14
JTClark
Senior Member
 
Join Date: Jan 2011
Location: Wisconsin
Posts: 199
JTClark is on a distinguished road
Default

gorilla will make a new brand and clear like water base and lightweight for fletching and insert someday who know ? it would be nice to see that ..
let see how company going to mmake for archery needed..
JTClark is offline   Reply With Quote
Old 02-07-2011, 01:28 PM   #15
Allen
Senior Member
 
Join Date: Feb 2006
Location: Maryland
Posts: 532
Allen is on a distinguished road
Default

The regular Gorilla Glue is useless for archery.

However, I've used the Gorilla Super Glue for fletching for about 2 years. It's cheaper and works as well as anything on the market at twice the price.

Lately, I've begun using Bohning tape for feathers. It's faster and does a much neater job. It sticks as good as any glue.

Hot melt for inserts. It's never failed me like epoxy has.

Allen
Allen is offline   Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 10:23 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2014, vBulletin Solutions, Inc.
Copyright 2004 3DShoots.com